What spalling is
Spalling is when the surface of concrete breaks away in flakes, chips or pits, leaving rough, exposed patches. A related problem, scaling, is the thin, widespread peeling of the top layer, commonly seen after freeze-thaw cycles and de-icing salts. The two overlap, and the repair approach is similar.
Why concrete spalls
- Freeze-thaw damage. Water gets into the concrete, freezes and expands, and over repeated cycles the surface breaks up.
- De-icing salts. These can make freeze-thaw damage worse, especially on concrete that wasn’t well finished or properly air-entrained.
- Corroding reinforcement. Rusting steel expands and pushes the concrete off. This is common where the steel is too close to the surface.
- Poor finishing or curing. Overworking the surface, adding water during finishing, or letting new concrete dry out too fast gives a weak top layer.
- Impact, heat or fire damage.
- Water and poor drainage. Constantly damp areas are most at risk.
Assess the damage first
- Tap test. Tap the area with a hammer or the handle of a chisel. A hollow or dull sound over a patch suggests it has separated from the concrete below, even if it looks intact.
- Check depth. Shallow flaking is much simpler to fix than deep spalls.
- Look for rebar. Exposed or rusted steel means deeper repair, and the corrosion needs treating.
- Check the extent. A few isolated spots suggest a patch. Widespread surface damage may suit an overlay. If the damage covers most of the slab, replacement may be better value. See is it cheaper to replace or repair concrete.
Repair step by step
Always read the repair product’s instructions and follow its limits on depth and temperature.
- Remove weak concrete. Chisel or grind away loose, flaking and hollow-sounding concrete until you reach solid material. Wear eye protection, gloves and a dust mask.
- Treat exposed steel. If rebar is exposed and rusty, clean off loose rust with a wire brush and treat it with a rust-inhibiting or protective coating, if the repair product’s instructions call for it. If steel is badly corroded or the damaged area is large, a professional or engineer should assess it.
- Clean. Sweep, vacuum and wash out dust, dirt and oil. Contaminants prevent bonding.
- Prepare the surface. Many cement-based products need a damp surface with no standing water, and some need a bonding agent or primer. Follow the label.
- Mix and place the repair material. A polymer-modified repair mortar or patching compound suits most patches, and a thin resurfacer suits widespread shallow spalling. See what to patch concrete with. Press it firmly in, level it with the surrounding surface and match the texture.
- Cure. Protect it from rapid drying, direct sun and frost, and give it the time the product says before traffic.
- Seal if appropriate. See the downsides of sealing concrete before choosing a sealer.
Choosing a repair method
- Isolated shallow pits and flakes: patching compound or repair mortar.
- Widespread shallow damage: a thin resurfacer or overlay. See can I resurface my concrete.
- Deep damage: a thicker repair mortar placed in layers, or a full-depth repair that removes the damaged concrete down to the base and replaces it, sometimes with reinforcement.
- Edges and corners: use a form to rebuild the shape. See repairing broken step edges.
- Vertical and overhead surfaces: use non-sag repair products.
How to stop it coming back
Fixing the cause is what stops a repeat:
- Improve drainage so water doesn’t pool or run onto the concrete.
- Avoid de-icing salts and chemicals on young or vulnerable concrete. Sand gives traction without the chemical effects.
- Seal exterior concrete if appropriate, and maintain the sealer.
- Repair small cracks promptly so water doesn’t get in. See our guide to concrete cracks.
- For new concrete, specify air-entrained concrete in freezing climates, and make sure it is finished and cured properly. Ask your supplier or designer.
- Keep joints in good condition.
When to call a professional
Call one if there is extensive rebar corrosion, spalling on structural elements (beams, columns, balconies, retaining walls), spalling on overhead surfaces, or if you are unsure about the cause. Falling concrete is a safety hazard.