Short answer: use mortar, not straight concrete
For most brick repairs, use mortar. Mortar is designed to bed bricks, bond to them, and sit between them. Concrete contains coarse aggregate, is usually harder and stiffer, and isn’t designed for thin joints or for filling a small hole between bricks.
Older, softer bricks and lime mortars especially can be damaged by a mortar that is much harder than the bricks, because the bricks end up taking the movement and stresses and may crack or spall. For historic or soft brickwork, a mortar matched to the original is a better idea. If the building is old or valuable, ask a mason.
Will concrete bond to brick?
It can stick, particularly if the brick is clean, rough and damp, but a bond isn’t the only consideration. Concrete shrinks as it dries, it is often stronger and less flexible than the surrounding masonry, and a thick fill in a hole can crack and separate. A bonding agent can help adhesion. For a small hole or a mortar joint, a bagged masonry mortar or a patching mortar made for masonry is a better option.
Choosing a patch material
- Bagged mortar mix (Type N or S in the US, or equivalent in other countries). Common for repointing and rebuilding joints. The right type depends on the wall and exposure, so check the bag and the age of the masonry.
- Pre-mixed patching or repair mortar. Convenient for filling holes and chips, and some come in colors.
- Hydraulic or quick-setting cement. Handy for small urgent jobs, but sets fast and hard.
- Brick-colored repair compounds or brick slips. For cosmetic fixes where appearance matters.
Color matching is difficult. Mix a small test batch, let it dry, since mortar usually dries lighter, and compare it to the wall.
Patching a hole in a brick wall
- Clear out the hole. Remove loose bricks, mortar and dust. Use a chisel or a brush.
- Check what’s behind it. Make sure there is something solid to fill against. For a hole through a wall, you may need to rebuild with bricks, or a backing.
- Dampen the area. Wet the surrounding brick lightly, so it doesn’t pull the water out of the patch. Avoid standing water.
- Mix the mortar to a stiff, workable consistency, like thick peanut butter.
- Fill in layers. Press mortar firmly in, working layers if the hole is deep, and let each stiffen slightly.
- Tool the surface to match the surrounding joints or surface, then brush lightly once it is firm.
- Cure slowly. Keep it damp for a couple of days and out of direct sun or frost.
Repointing cracked or crumbling mortar joints
Repointing means replacing damaged mortar in the joints. For tools and technique in more depth, see how to repoint a brick wall.
- Rake out the old mortar to a depth around two to three times the joint width, or about 1/2 to 1 inch, without damaging the bricks. A hand tool is safer than an angle grinder for beginners.
- Brush and vacuum out dust.
- Dampen the joints.
- Pack new mortar firmly into the joints in layers, using a pointing tool or small trowel.
- Tool the joints to match the profile of the originals once the mortar is thumbprint-hard.
- Brush off excess and cure slowly.
Replacing damaged bricks
If a brick is cracked or crumbling, chisel out the mortar around it, remove it, clean the cavity, and bed a replacement brick in fresh mortar on all sides. Wear eye protection, since chips fly. If the wall is structural or you see widespread cracking or bulging, get a professional to look at it. See also shrinkage cracks in block walls.
How long does repointing last?
It depends on the mortar, the exposure, the quality of the work and the condition of the bricks. Well-done repointing can last for decades, but I wouldn’t promise a number. If mortar keeps failing, check for moisture problems. See waterproofing basement and brick walls and removing efflorescence.
Mistakes to avoid
- Using a mortar much harder than the bricks.
- Smearing mortar over the face of the brick instead of keeping it in the joint.
- Filling only the surface of a deep joint.
- Skipping dust removal and dampening.
- Working in freezing temperatures or full sun.
- Sealing a wall that is wet from behind.