When does a wall need repointing?

Repointing means removing deteriorated mortar from the joints and replacing it with fresh mortar. It is also called tuckpointing. Look for:

  • Crumbling or powdery mortar
  • Holes and cracks in the joints
  • Mortar eroded back from the face of the brick (a commonly used guide is more than about 6 mm or ¼ inch)
  • Joints separating from the bricks
  • Plants growing in the joints

Repointing is a maintenance job, not a cure for structural cracks or bulging walls. If the wall is moving or leaning, get a structural opinion first. If you are trying to stop water getting in, check first that the problem really is the joints; see what happens when water gets behind brick and waterproofing basement and brick walls.

Tools and materials

  • Mortar rake or plugging chisel and a hammer. Some people use a wheeled joint raker or an angle grinder with a suitable blade, but a grinder can easily damage brick edges.
  • Stiff brush and a masonry brush
  • Hawk (a flat board for holding mortar) and a pointing trowel
  • Jointing tool, or trowel, to shape the joints
  • Bucket, hose or garden sprayer
  • Drop cloths
  • Safety glasses, gloves and a dust mask or respirator

Safety: raking out old mortar creates fine dust, which can contain silica. Wear a suitable mask, and consider wetting the wall lightly to reduce dust. Fresh cement and lime mortar is caustic to skin, so wear gloves. For high walls and chimneys, use proper access equipment, or hire a professional.

Choose the right mortar

The new mortar should be no harder than the brick, ideally a little softer, so that any movement and moisture pass through the joints rather than damaging the bricks.

  • For most modern walls, a mortar such as a US Type N or O, or a UK mix of around 1 : 5 or 1 : 6 cement : building sand with plasticiser is typical. See mortar mix ratios and Type S versus Type N.
  • For old, soft bricks and historic walls, a lime mortar is usually recommended. A hard cement-rich mix can cause old bricks to crumble beside the joint.
  • Match the colour and sand as closely as you can on a test patch; new mortar will look different from weathered mortar, particularly if you only repoint part of a wall.

How to repoint step by step

  1. Choose the right weather. Avoid frost, heavy rain and very hot sun. Many mortar bags specify a temperature range (roughly 4°C to 38°C, or 40°F to 100°F), so check yours.
  2. Protect the surroundings with drop cloths.
  3. Rake out the old mortar to a depth of about twice the joint width, commonly 15 to 20 mm (about ½ to ¾ inch) for typical joints. Do the vertical joints first and then the horizontal ones, working from the top down. Avoid damaging the bricks.
  4. Brush out the joints to remove dust and loose material.
  5. Dampen the joints lightly so the dry bricks do not pull water out of the new mortar. There should be no standing water.
  6. Mix the mortar in small batches to a stiff, workable texture, often compared to peanut butter. See mortar consistency.
  7. Fill the joints. Press mortar firmly in using the hawk and pointing trowel. Fill the horizontal joints first and then the vertical, or follow your preferred order, in layers if the joint is deep, so the mortar is well compacted and there are no voids.
  8. Tool the joints once the mortar has stiffened enough that a thumbprint barely marks it, usually after about 30 to 45 minutes depending on the weather. Use a jointing tool to match the profile of the surrounding joints.
  9. Brush off the excess lightly with a soft brush once the mortar has set a little, without digging into the joints.

Joint profiles

Common profiles are flush, concave (bucket handle), and weathered or struck. Concave and weathered joints tend to shed water well. Deeply recessed joints can collect water and are not usually recommended in exposed locations.

Aftercare

Keep new pointing from drying too fast: mist it lightly during the next few days in warm weather, and protect it from rain and frost. See curing brickwork for details.

Common mistakes

  • Using a mortar that is harder than the bricks.
  • Cutting into the brick edges with a grinder.
  • Not raking deep enough, so the new mortar lacks the depth to hold.
  • Smearing mortar over the brick faces.
  • Working too big an area at once so the mortar dries before it is tooled.
  • Repointing only part of a wall and expecting a perfect match.

When to hire a professional

Large areas, high walls, chimneys, historic or listed buildings and walls with structural problems are often best left to an experienced mason. Repointing is straightforward in principle but slow, labour-intensive work, and the quality of the finish and the choice of mortar matter.