Concrete Repair

Shrinkage Cracks in Concrete Block Walls

Why concrete block walls develop shrinkage cracks, how to tell them from structural cracks, how to repair them, and how to prevent them in new walls.

On this page
  1. What shrinkage cracks in block walls look like
  2. Why block walls crack as they dry
  3. Shrinkage crack or something more serious?
  4. How big a crack is acceptable?
  5. How to repair a crack in a block wall
  6. How to prevent shrinkage cracks
  7. Video tutorials

What shrinkage cracks in block walls look like

Shrinkage cracks in concrete block (CMU) walls are typically thin and fairly regular. They often follow the mortar joints in a stepped pattern, or run vertically, sometimes through the full height of the wall, and they often appear at weak points such as above and below openings, near corners, or where the wall changes height or thickness.

They tend to show up in the first months to a couple of years after construction, as the blocks, mortar and grout finish drying and the wall adjusts to its environment.

Why block walls crack as they dry

Concrete products shrink slightly as they lose moisture. A block wall is restrained by its footing, by the floor or roof, and by crossing walls, so it can’t shrink freely. The stress concentrates at weak points, and the wall cracks. Contributing factors include:

  • Blocks that were very wet or not allowed to dry when laid.
  • No control joints, or control joints in the wrong places.
  • Long wall runs without movement joints.
  • Strong, stiff mortar mixes, or poor bond.
  • Rapid drying in hot, windy weather, or weather swings.
  • Little or no horizontal joint reinforcement.

Shrinkage crack or something more serious?

Shrinkage cracks are usually thin and stable. Signs that a crack may be something else include:

  • It is wide, or getting wider.
  • The wall is bowing, leaning or displaced, or the two sides of the crack sit at different levels.
  • Diagonal cracking from corners of doors, windows or the base of the wall.
  • Cracks accompanied by sticking doors, uneven floors or gaps at the base of the wall.
  • Water pushing through, particularly in a retaining or basement wall.

Cracks like these can point to settlement, soil pressure, or structural issues, and are worth having a structural engineer inspect before you patch anything. For general slab and foundation guidance, see our guide to cracks in concrete slabs and foundations.

How big a crack is acceptable?

No single limit fits every wall. Hairline cracks that are stable are widely treated as cosmetic, while a crack that is wide enough to insert a coin, or one that is growing, merits a closer look. Retaining walls, basement walls and anything holding back soil or water have tighter expectations than a garden wall. Mark the ends of a crack and measure it over a few weeks to see whether it is moving.

How to repair a crack in a block wall

Wait until the crack has stopped moving if you can. Then:

  1. Clean the crack. Brush out loose mortar and dust with a wire brush, and blow or vacuum it clean.
  2. Choose the filler. For fine, stable cracks, a flexible masonry or elastomeric sealant or a masonry crack filler is common. It tolerates small movements better than rigid mortar. For wider cracks in mortar joints, raking out the joint and repointing with fresh mortar is typical.
  3. Fill the crack. For sealant, gun it in and tool it flush. For mortar, dampen the surrounding masonry lightly, pack the joint firmly in layers, and tool it to match.
  4. Cracks through the blocks. Rigid patching products or masonry repair mortars can be used, but they may crack again if the wall keeps moving. A flexible sealant is more forgiving for small cracks.
  5. Finish. Paint or coat the wall afterwards if you like. Use a masonry-appropriate paint or elastomeric coating that bridges fine cracks.

If water comes through, address the moisture too. See waterproofing basement and brick walls. For repointing and replacing damaged units in brick, see patching a brick wall.

How to prevent shrinkage cracks

For new walls, these practices are widely recommended:

  • Control joints at suitable intervals and at points of weakness, such as near openings and changes in wall height. Your designer or local code will specify the layout.
  • Horizontal joint reinforcement in the mortar bed courses, if specified.
  • Keep blocks dry on site, covered and off the ground, and use units that have been allowed to cure and dry as the supplier advises.
  • Use an appropriate mortar for the job, and don’t over-wet the mix.
  • Protect the wall in extreme weather, avoiding rapid drying in hot, windy conditions.
  • Make sure footings are sound so the wall isn’t settling.

Video tutorials

If you prefer watching, search for videos on repairing block wall cracks and masonry crack repair from established tool and masonry channels. Look for ones that show cleaning the crack, filler choice and finishing, and be cautious with any video that skips working out why the crack formed.

If you also see white deposits along the wall, they’re likely salts left by moisture. See removing efflorescence.