Short answer
A widely used rule of thumb is to space control joints at roughly 24 to 36 times the slab thickness, and to cut them to about one quarter of the slab thickness. For a 100 mm (4 in) slab, that works out to joints roughly every 2.4–3.6 m (8–12 ft), cut about 25 mm (1 in) deep. Panels should be as close to square as practical. These are general guidelines, and project specifications or an engineer’s design take priority.
Why concrete needs joints
Concrete shrinks slightly as it dries and cools, and it expands and contracts with temperature. Because the slab is restrained by the ground and by its own size, it develops tension and cracks. Control joints create deliberate lines of weakness so the cracks form in straight, tidy lines within the joint instead of randomly across the surface. They reduce cracking but cannot guarantee there will be none; for cracks that do appear, see cracks in concrete slabs and how to fix them. Steel doesn’t replace joints; see rebar or wire mesh in a concrete slab.
Spacing rule of thumb
Multiply the slab thickness by 24 to 36 (in the same units) to get the maximum joint spacing. The lower end is safer, especially for unreinforced slabs, thin slabs, mixes with high shrinkage or outdoor slabs exposed to the weather.
| Slab thickness | Spacing at 24× | Spacing at 36× |
|---|---|---|
| 75 mm (3 in) | 1.8 m (6 ft) | 2.7 m (9 ft) |
| 100 mm (4 in) | 2.4 m (8 ft) | 3.6 m (12 ft) |
| 125 mm (5 in) | 3.0 m (10 ft) | 4.5 m (15 ft) |
| 150 mm (6 in) | 3.6 m (12 ft) | 5.4 m (18 ft) |
In the imperial version, this is often given as 2 to 3 feet of spacing for every inch of thickness. Some specifications use tighter spacings for driveways or exposed slabs, so check the design.
How deep to cut
Joints are usually cut or formed to at least one quarter of the slab thickness (some guidance says one quarter to one third). For a 100 mm slab, that is about 25 mm. If the cut is too shallow, the slab may crack elsewhere instead.
Layout tips
- Keep panels roughly square. As a rule of thumb, the long side shouldn’t exceed about 1.5 times the short side.
- Avoid narrow strips and awkward shapes, which tend to crack.
- Run joints into corners. Cracks tend to start at re-entrant (inward-pointing) corners, such as around the corner of a house, a column or a drain, so place joints that run out from them.
- Line joints up with any joints in adjoining slabs or paving, and with edges of doors or posts, for a neater result.
- For paths, which are narrow, cross-joints at intervals of around 1.5–3 m are common, depending on width and thickness. See how thick a concrete path needs to be.
When and how to make joints
- Tooled joints: formed in the wet surface with a grooving tool guided against a straight board, once the concrete has been floated. Easy for small DIY slabs, though the tool can leave a shallower groove than a cut.
- Saw-cut joints: cut with a concrete saw shortly after the concrete has hardened enough not to ravel, but before shrinkage cracks start. Depending on temperature and mix, that is often within roughly 6–18 hours, though early-entry saws can cut sooner. Check the saw maker’s guidance, and don’t leave it too long.
- Inserted strips: plastic or hardboard strips can be set into the fresh concrete.
Other joint types
- Control (contraction) joints are the ones above, creating planned cracks.
- Construction joints are where one pour stops and the next begins, such as when pouring in sections. They are often tied with dowels or bars, or formed with a keyway, and they may double as control joints. See how to lay a concrete slab.
- Isolation (expansion) joints separate the slab from walls, columns, steps and other fixed elements so they can move independently. They’re commonly formed with compressible filler board.
Common mistakes
- Spacing joints too far apart.
- Cutting too shallow, or too late.
- Making panels long and narrow.
- Not isolating the slab from the building or fixed elements.
- Poor curing, which increases shrinkage cracking; see curing concrete.
- Ignoring slab base quality, since weak support contributes to cracking.